Features:
UNS Number N08825
Incoloy 825 has excellent resistance to chloride-ion-induced stress corrosion cracking, reducing environments containing phosphoric and sulfuric acids, oxidizing environments containing nitric acid and nitrates, and pitting, crevice corrosion and intergranular corrosion. It has good mechanical properties at cryogenic temperatures to moderately high temperatures up to 538℃.
Applications:
Chemical process industry, acid production, pickling equipment, pollution control equipment.
Products of Incoloy 825 available
• Sheet
• Plate
• Bar
• Pipe & Tube (welded & seamless)
• Fittings (i.e. flanges, slip-ons, blinds, weld-necks, lapjoints, long welding necks, socket welds, elbows, tees, stub-ends, returns, caps, crosses, reducers, and pipe nipples)
		
			• Wire
		
		
			
 
		
		
			Incoloy 825 Chemical composition: 
		
		
			
				
					| 
						Alloy
					 | 
					
						%
					 | 
					
						Ni
					 | 
					
						Cr
					 | 
					
						Fe
					 | 
					
						C
					 | 
					
						Mn
					 | 
					
						Si
					 | 
					
						Cu
					 | 
					
						Mo
					 | 
					
						Al
					 | 
					
						Ti
					 | 
					
						P
					 | 
					
						S
					 | 
				
			
			
				
					| 
						825
					 | 
					
						Min.
					 | 
					
						38
					 | 
					
						19.5
					 | 
					
						balance
					 | 
					
					 | 
					
					 | 
					
					 | 
					
						1.5
					 | 
					
						2.5
					 | 
					
						1.0
					 | 
					
						0.6
					 | 
					
					 | 
					
					 | 
				
				
					| 
						Max.
					 | 
					
						46
					 | 
					
						23.5
					 | 
					
						balance
					 | 
					
						0.05
					 | 
					
						1
					 | 
					
						0.5
					 | 
					
						3
					 | 
					
						3.5
					 | 
					
						0.2
					 | 
					
						1.2
					 | 
					
						0.02
					 | 
					
						0.03
					 | 
				
			
		
Incoloy 825 Physical properties: 
		
			
				
					| 
						Density
					 | 
					
						8.1 g/cm³
					 | 
				
				
					| 
						Melting range
					 | 
					
						1370-1400℃
					 | 
				
			
		
Incoloy 825 Alloy mi nimum mechanical properties in the room temperature: 
		
			
				
					| 
						Alloy state
					 | 
					
						Tensile strength Rm N/mm²
					 | 
					
						Yield strength R P0. 2N/mm²
					 | 
					
						Elongation A 5 %
					 | 
					
						Brinell hardness HB
					 | 
				
				
					| 
						825
					 | 
					
						550
					 | 
					
						220
					 | 
					
						30
					 | 
					
						≤200
					 | 
				
			
		
ASTM Specifications
		
			
				
					| 
						Pipe Smls
					 | 
					
						Sheet/Plate
					 | 
					
						Bar
					 | 
					
						Forging
					 | 
					
						Fitting
					 | 
				
			
			
				
					| 
						B423
					 | 
					
						B424
					 | 
					
						B425
					 | 
					
						B564
					 | 
					
						B366, B564
					 |